Orion 930: Get to Know the Orion Moisture Meter
You may also like
Last updated on December 11th, 2025
The Orion® line of wood moisture meters continues Wagner’s 50-plus year tradition of providing accurate, dependable non-damaging pinless moisture measurement technology, measuring IN the wood not just ON the wood.
Jason Spangler, Flooring Division Manager for Wagner Meters, introduces the Orion 930 Dual Depth Pinless Wood Moisture Meter and demonstrates the ease of choosing deep or shallow depth reading capabilities as well as the quick and easy on-site calibration process.
Last updated on December 11th, 2025
| Cookie | Duration | Description |
|---|---|---|
| cookielawinfo-checkbox-analytics | 11 months | This cookie is set by GDPR Cookie Consent plugin. The cookie is used to store the user consent for the cookies in the category "Analytics". |
| cookielawinfo-checkbox-functional | 11 months | The cookie is set by GDPR cookie consent to record the user consent for the cookies in the category "Functional". |
| cookielawinfo-checkbox-necessary | 11 months | This cookie is set by GDPR Cookie Consent plugin. The cookies is used to store the user consent for the cookies in the category "Necessary". |
| cookielawinfo-checkbox-others | 11 months | This cookie is set by GDPR Cookie Consent plugin. The cookie is used to store the user consent for the cookies in the category "Other. |
| cookielawinfo-checkbox-performance | 11 months | This cookie is set by GDPR Cookie Consent plugin. The cookie is used to store the user consent for the cookies in the category "Performance". |
| viewed_cookie_policy | 11 months | The cookie is set by the GDPR Cookie Consent plugin and is used to store whether or not user has consented to the use of cookies. It does not store any personal data. |
Hi I’m considering buying the Orion 930. May I know what is its minimum and maximum moisture content measurement? I actually will be using it to measure fungal mycelia block. Do you think it will work?